D 802 EDCoCr-A-03 HRc38-47. Resistance to heat, wear and corrosion. Hardfacing of high temperature part such as the edge of thermo-cutter.
HRc38-47,耐热、耐蚀、耐磨。堆焊高温工件如热剪切刀刃 ECoCr-A
D 812 EDCoCr-B-03 HRc45-50. Resistance to heat, wear and corrosion. Hardfacing of high temperature part such as internal-combustion engine valve.
HRc45-50,耐热、耐蚀、耐磨。堆焊高温工件如内燃机阀 ECoCr-B
D 822 HRc≥53. Resistance to Wear and heat, bad shock resistance. Hardfacing of rotating blade wheel of boiler.
HRc≥53,耐热、耐磨,但抗冲击性差。堆焊锅炉旋转叶轮
D 832 EDCoCr-C-03 HRc≥50. Wear and heat resistance. Hardfacing of high temperature part such as hot-rolling guided way.
HRc≥50,耐热、耐磨。堆焊高温工件如热轧导轨 ECoCr-C
D 842 EDCoCr-D-03 HRc28-38. Corrosion and thermo-fatigue resistance, work harding. Hardfacing of hot forging die.
HRc28-38,耐蚀、抗热疲劳,具有加工硬化性。堆焊热锻模
HRc38-47,耐热、耐蚀、耐磨。堆焊高温工件如热剪切刀刃 ECoCr-A
D 812 EDCoCr-B-03 HRc45-50. Resistance to heat, wear and corrosion. Hardfacing of high temperature part such as internal-combustion engine valve.
HRc45-50,耐热、耐蚀、耐磨。堆焊高温工件如内燃机阀 ECoCr-B
D 822 HRc≥53. Resistance to Wear and heat, bad shock resistance. Hardfacing of rotating blade wheel of boiler.
HRc≥53,耐热、耐磨,但抗冲击性差。堆焊锅炉旋转叶轮
D 832 EDCoCr-C-03 HRc≥50. Wear and heat resistance. Hardfacing of high temperature part such as hot-rolling guided way.
HRc≥50,耐热、耐磨。堆焊高温工件如热轧导轨 ECoCr-C
D 842 EDCoCr-D-03 HRc28-38. Corrosion and thermo-fatigue resistance, work harding. Hardfacing of hot forging die.
HRc28-38,耐蚀、抗热疲劳,具有加工硬化性。堆焊热锻模